Oct 25, 2013 #1 dlkg Mechanical Joined Feb 21, 2005 Messages 3 Location US When performing macros on fillet welds - does ASME or AWS allow you to mount the macros? Any help would be appreciated. Thanks
When performing macros on fillet welds - does ASME or AWS allow you to mount the macros? Any help would be appreciated. Thanks
Oct 25, 2013 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Yes, provided the entire fillet weld is captured and can be examined for complete fusion and no cracks. Upvote 0 Downvote
Yes, provided the entire fillet weld is captured and can be examined for complete fusion and no cracks.