I am working on WPS and PQR for canister lid welding and have some questions about the test coupon preparation. The wall thickness of the canister structure lid is 3" wall thickness (which will weld to the outer shell of the canister) and have a 30° bevel angle with 1.25" deep. But the weld penetration requirement is 1". My questions are:
1. Base on ASME IX,QW-451, I will need a 1.5" test coupon to qualify the 3" thickness base metal, is that right? or the base metal thickness can be treated as 1.25" and I can use an 5/8" thick test coupon?
2. If I use 1.5" thick test coupon, should I prepare the bevel as deep as 1.5" or I can make 1.25" deep bevel?
I really hope I can get some help on this and your reply is highly appreciated.
1. Base on ASME IX,QW-451, I will need a 1.5" test coupon to qualify the 3" thickness base metal, is that right? or the base metal thickness can be treated as 1.25" and I can use an 5/8" thick test coupon?
2. If I use 1.5" thick test coupon, should I prepare the bevel as deep as 1.5" or I can make 1.25" deep bevel?
I really hope I can get some help on this and your reply is highly appreciated.