DEar All,

Could you please advise me please any link / resource where i can find examples of piping composite wrapping (temporary repair) calculations ?
How many layers depending of piping / fluid parameters ... In fact PCC-2 practical application examples

Tank you so much
 
Is there nothing in ISO 24817 to support?
 
I think this is more of a vendor dependant thing than a calculation per se.

What are you trying to calculate exactly and why?

Composite wrap is only for non through wall thickness corrosion.
 
I will suggest you to look to the book ; Rehabilitation of Pipelines Using Fiber-reinforced Polymer (FRP) Composites by Vistasp M. Karbhari

If you write ' Rehabilitation of Pipelines composite ' and search the web some of the outcomes ;
www.compositerepair.org : there are useful articles at this site

 
See the latest PCC-2. There are entire Chapters/Articles devoted to temp pipe wrap design.
 
I think this is more of a vendor dependant thing than a calculation per se.

What are you trying to calculate exactly and why?

Composite wrap is only for non through wall thickness corrosion.
There were some perforations pin-hole leaks in piping and to calculate number of wraps depending what wrap it is ....
 
AFAIK, composite wreaks are not designed for through wall defects.

You needs a metallic clamp or sleevev. Or cut put.
 