Hello,

I've a pressure vessel designed according to ASME VIII Div.1, material P9 (PN°5B for ASME IX). Main shell is a seamless piepe SA 335 P9.

According to SA 335 from ASME II PART.A, base material shall be furnished normalized and tempered at minimum 675°C.

Now this vessel, in accordance with ASME VIII Div.1, shall be also PWHT.

According to Table UCS-56-4, minimum temperature of PWHT is 675°C...and this is strange, because many inspectors told me that PWHT tempering temperature shall be at least 30°C below the tempering temperature of base material.

I don't find this last request in any point of ASME VIII Div.1. What's your opinion?

Good practice and old european codes suggest to follow this requirement, but I don't know if this point is covered anywhere in ASME.

Thank you.

 
Follow the Code minimum requirements. Look at the minimum UTS of this material. It is easily met with the additional PWHT.
 
Yes, this alloy should have plenty of margin to PWHT at the min temper temp.
It wouldn't surprise me if the original temper wasn't well above this temp. (as I recall 725C is common)
There is a lot of work that has been done on this grade for optimizing different properties (strength, toughness, creep).
A bunch of the EPRI reports are available to the public on P9 and P91.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
EdStainless said:
A bunch of the EPRI reports are available to the public on P9 and P91.

Where exactly? I can't find anything...thank you
 