Metalmeister
Nuclear
Does anyone have knowledge or experience with temperbead overlay weld qualification per Code Case N638.
Is it OK to treat this PQR depicted in the code case as a partial penetration groove weld and cut off the bottom at the fusion line and discard the bottom, and only side bending the portion with the weld? I know that one can do this with a normal partial pen groove weld, but can you do this on a temperbead weld qual, or do you have to side bend the entire plate thickness which is typically about 2-3 inches?
Is it OK to treat this PQR depicted in the code case as a partial penetration groove weld and cut off the bottom at the fusion line and discard the bottom, and only side bending the portion with the weld? I know that one can do this with a normal partial pen groove weld, but can you do this on a temperbead weld qual, or do you have to side bend the entire plate thickness which is typically about 2-3 inches?