danielmurray
Electrical
- Dec 26, 2002
- 8
We use several different methods for monitoring the condition of the insulation in our motors. One method in use is a spot check. I am having a difficult time finding the correct temperaure correction factor for Class H insulation in rotating equipment. I have a chart for Class A and B. Can anyone help?