Is temper bead welding allowed per this spec. to be performed instead of PWHT? I know it is allowed per NACE MR0103, but I cannot find it in this spec.?
 
Replies continue below

Recommended for you

NACE MR0175 only deals with materials and hardness requirements for SSC and SCC resistance for petrochemical environments. If temper bead welding can result in permitted hardness values this should be acceptable.
 
What is the component and material to be welded with temper bead technique ? Note meeting the hardness values to MR-0175(in weld,HAZ) are not easy.Hence a lot of variable are to be considered.

Appreciate you response.

Thanks

Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299


 