We've performed a PWHT cycle on a vessel (P1 material, 3/8" THK, 20" OD, 30ft long). The temp ramp exceeded the Code specified allowable of 400deg F/hr (max rate seen was 575 F/hr for ~15min, while the avg rate from 800F to 1150F was 300 F/hr). At no point did the other parameters of the PWHT fall outside Code allowables. Is there a method to prove acceptance of this PWHT cycle to the AI, or is the only option to redo the cycle (we are not limited by the WPSs to only one PWHT)? Thank you.