Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

tek screw drill point sizes 1

Status
Not open for further replies.

hinged

Mechanical
Joined
Jun 6, 2002
Messages
22
Location
US
WHere can you find the required drill point diameter for self drilling tek screws?
 
?? self drilling = no need for a drill bit as the screw has their own drill point as part of the fastener.
 
mcgyvr,

thank you, but what I'm looking for is the drill point diameter of the self drilling screw.

hinged
 
Buy a screw,
Take a caliper or a micrometer and measure it.
B.E.
 
You might request a CAD model from the mfr, as well.
 
I understand that the question is along the lines of when can you use a screw with a #1 point; when do you have to use a #2 instead of a #1, when do you have to use a #3 instead of a #2, right? Here's what the Cold-Formed Steel Engineers Association has to say in Tech Note TN-565c:

Format:
nominal screw size / maximum recommended total thickness of steel sheets

For #2 Point Style
4 / 0.080"
6 / 0.090"
8 / 0.100"
10 / 0.110"
12 / 0.140"
1/4" / 0.175"

For #3 Point Style
6 / 0.090"-0.110"
8 / 0.100"-0.140"
10 / 0.110"-0.175"
12 / 0.110"-0.210"
1/4" / 0.110"-0.210"

I don't know why the #3 point style data is given in a range, while the #2 gives a single value. Evidently #1 points are for very light connections and are not worth including in this table. Suggest you obtain TN-565c -- I belong to the association, and I can not recall if it is free or for a charge.
 