Oct 6, 2003 1 #1 etek39 Chemical Joined Dec 11, 2002 Messages 2 Location US I am looking to bond teflon with metal. I am looking for a U.S. supplier of sodium etch solution for Teflon. Please help with name, telephone. Etek 39
I am looking to bond teflon with metal. I am looking for a U.S. supplier of sodium etch solution for Teflon. Please help with name, telephone. Etek 39
Oct 13, 2003 #2 tothepoint Mechanical Joined Mar 31, 2003 Messages 91 Location US W.L. Gore & Assoc., Inc. manufactures and markets a product called "Tetra Etch". This is a sodium etching solution as you describe. Gore's corporate headquarters is in Newark, DE. Upvote 0 Downvote
W.L. Gore & Assoc., Inc. manufactures and markets a product called "Tetra Etch". This is a sodium etching solution as you describe. Gore's corporate headquarters is in Newark, DE.