Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for an ABS to Rubber solution.

Status
Not open for further replies.

ShaneDoe

Mechanical
Dec 19, 2012
10
I am needing to attach a seal to ABS, the Seal material is still up in the air but rubber / silicone are very likely. Is there any chemical solvents that will hermetically attach ABS to Rubber or the like and hold while under 80psi of pressure?

Thanks
 
Replies continue below

Recommended for you

Acetone and MEK are used to solvent bond ABS to itself. I imagine there is an elastomer that can be dissolved with these solvents, though I am not sure they are suitable for your seal application.

If you choose to use an actual adhesive material, here is a design guide from Henkel:

 