Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Tapping 0-80 blind holes in Tungsten alloy

Status
Not open for further replies.

Makule

Geotechnical
Aug 21, 2008
1
Anyone out there have any experience in machining (tapping) extremely small holes 00-96, 0-80 in "W" material.. non magnetic alloy? I know I wish it was CuW too! Thanks
 
Replies continue below

Recommended for you

We do lots of this kind of thing. Sadly I'm in design and it's done by a vendor so I don't know details.

I do know they have a pig of a time doing them to any depth.

I think our vendor is 'Next Intent' if that's any help.

KENAT, probably the least qualified checker you'll ever meet...
 
Status