Hello,
With regards to hydro testing of tanks which had undergone major repairs like bottom or shell plates replacements, how can I calculate the test pressure for a tank with the following design data:
- Crude Oil Fixed Doom Roof Tank
- Construction Code: API 650 Appendix F
- Design Pressure/Vaccum: 3.45 kPag / 0.5 kPag (51 mmH2O)
- Working Pressure: 0.9 to 1.5 kPag
- Max. Operating Temperature: 90 degrees Celsius.
Or, it is enough to fill the Tank to the maximum liquid level.
Additionally, how many hours shall be the duration of the test?
Thank you.
With regards to hydro testing of tanks which had undergone major repairs like bottom or shell plates replacements, how can I calculate the test pressure for a tank with the following design data:
- Crude Oil Fixed Doom Roof Tank
- Construction Code: API 650 Appendix F
- Design Pressure/Vaccum: 3.45 kPag / 0.5 kPag (51 mmH2O)
- Working Pressure: 0.9 to 1.5 kPag
- Max. Operating Temperature: 90 degrees Celsius.
Or, it is enough to fill the Tank to the maximum liquid level.
Additionally, how many hours shall be the duration of the test?
Thank you.