Hi,
Refer to attached photo
I need to decide whether to tack weld a hex bolt head or hex nut ? . The reason being is the design of mounting bolt is meant to be drop down with hex head at the bottom, however it seems there is accessibility issue for the maintenance to access the spanner from confined space from bottom. Furthermore, this skid is going to be fully grouted with the foundation.
I am considering the following option:
1. Tack weld the head from the bottom
2. Tack weld the Nut from the bottom
Option 1: It was preferable to just do a tack welding, I am intending to do 3 point tack weld.
1 where should be the location of tack weld on hex head to prevent snapping during torquing?
2 Do you think the tack weld could alter the structure of the Mild steel ?
Option 2: Tack weld the nut from the bottom
Issue: risk of splatter ruin the thread, If this has to be done, we are going to tighten bolt and nut, after that maybe use 1 more nut to cover the threads.
In this case, if we are fully grout, We are going to have issue of breaking the thread too, as bottom of the C channel would be fully grout and the thread could have come into contact with the grouts.Upon grouting, if there threads ruined, there is difficulties in replacing the nuts. What is your view on this.
if nut at the bottom, should we full weld or tack weld few points ?
Option 3 : No weld at all just fully grout the Hex head ( 1 inch thickness to the fully grouted), however I do not think, there is sufficient strength to hold tight the bolt preventing from rotating upon tightening the equipment
What are the considerations for welding 2 materials, My skid is mild steel and the bolt and nut is galvanized steel.
Refer to attached photo
I need to decide whether to tack weld a hex bolt head or hex nut ? . The reason being is the design of mounting bolt is meant to be drop down with hex head at the bottom, however it seems there is accessibility issue for the maintenance to access the spanner from confined space from bottom. Furthermore, this skid is going to be fully grouted with the foundation.
I am considering the following option:
1. Tack weld the head from the bottom
2. Tack weld the Nut from the bottom
Option 1: It was preferable to just do a tack welding, I am intending to do 3 point tack weld.
1 where should be the location of tack weld on hex head to prevent snapping during torquing?
2 Do you think the tack weld could alter the structure of the Mild steel ?
Option 2: Tack weld the nut from the bottom
Issue: risk of splatter ruin the thread, If this has to be done, we are going to tighten bolt and nut, after that maybe use 1 more nut to cover the threads.
In this case, if we are fully grout, We are going to have issue of breaking the thread too, as bottom of the C channel would be fully grout and the thread could have come into contact with the grouts.Upon grouting, if there threads ruined, there is difficulties in replacing the nuts. What is your view on this.
if nut at the bottom, should we full weld or tack weld few points ?
Option 3 : No weld at all just fully grout the Hex head ( 1 inch thickness to the fully grouted), however I do not think, there is sufficient strength to hold tight the bolt preventing from rotating upon tightening the equipment
What are the considerations for welding 2 materials, My skid is mild steel and the bolt and nut is galvanized steel.