I am living in Singapore.

I am looking for the above for calculations purposes.
would any of you please provide me the above.
Thanks.
 
Not sure what tropical species you are looking for, but a good resources can be found at the Forest Products Laboratory's website. The Wood Handbook Chapter 4 I believe would be helpful. You may download the chapter free in *.pdf format.

 
Try the following books conference notes - Timbers of Sabah by Burgess ..or Tropical Timber of the World Or Indonesian Wood Atlas Vol 1 (English Translation avialable), Timbers of SE Asia, or proceedings from KL conference on Tropical Hardwoods.

These may be available from your local Technical Library.
 