No, the values in this table cannot simply be interpolated like the relationship between temperature and allowable stress values. Table 39.1 is a time/temperature relationship derived from a parametric equation, similar to the Larson-Miller creep equation. For interpolation you would need to know the actual equation and constant to determine a time, based on a known PWHT.