keyPitsimplE
Structural
- Aug 5, 2008
- 104
Referencing thread337-254770
I am designing a lumber diaphragm using NDS Table 4.2C for 2x6 T&G Horiz Lumber Sheathing and seeing an allowable shear value of 50 plf. This is fine with me, but there is no indication anywhere in the NDS that I can find that dictates the maximum spacing of the supports. Naturally there is a limit for vertical loads, but none is given for lateral. Mine happen to be about 6' apart, some smaller. I only have a 25 psf snow load.
I would rather not put plywood on the top because I think it is a waste of money for this project. It is a small residential building, roof only. We are adding on and matching the existing.
Any thoughts?
Thanks,
I am designing a lumber diaphragm using NDS Table 4.2C for 2x6 T&G Horiz Lumber Sheathing and seeing an allowable shear value of 50 plf. This is fine with me, but there is no indication anywhere in the NDS that I can find that dictates the maximum spacing of the supports. Naturally there is a limit for vertical loads, but none is given for lateral. Mine happen to be about 6' apart, some smaller. I only have a 25 psf snow load.
I would rather not put plywood on the top because I think it is a waste of money for this project. It is a small residential building, roof only. We are adding on and matching the existing.
Any thoughts?
Thanks,