We are currently applying ED coating to driven sprockets. During the salt spray test, we observed signs of red corrosion that appeared prior to meeting the customer's specifications. We would appreciate any helpful advice on enhancing the durability of the ED coating.
 
Plating solution, electrode material, voltage, current, fluid temperature, bath dimensions, etc.

Are you plating one item, are many at once?
 
Sharp corners.
 