Dear All,
We have to supply the SA213-316L & TP321 U tubes for our U type exchangers, (OD 19.05 x Thk 1.65 avg mm) under ASME code.
Now client has asked to apply for “Supplementary Requirement” per SA213, S1 and S2 as per grade.
When I asked my tube maker for the same, most of them suggest it is not possible mainly S1.2 heat treatment after roll straightening.
Their argument is, after heat treatment, tube shape will not be straight. Which is why they do straightening process after heat treatment.
some of them are not recommended to doing it this because of wall thickness is thin, as S1 doesn't allow any mechanical straightening operation after stress relief annealing
so they are not confident about problems occur during installation of un straightened U-Tubes into baffles and tube sheets.
So my question is, Is it practical to perform S1 or S2 Supplementary Requirement, as we have heat treated the tubes as per table 3 of SA213 ASME Sec II-A.
I am not sure how it will affect in fabrication as tubes delivered after stress relief process .
Please advise.