Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Suitability of ASTM A216 Gr WCB for service

Status
Not open for further replies.

Tatts

Mechanical
Aug 26, 2009
1
Is there a decent site that will allow me to assess suitability of WCB for use with certain media in pipeline systems and valves?
 
Replies continue below

Recommended for you

ASTM STANDARD RELATED BOOK TO STEEL PIPING, TUBING,& FITTINGS WILL BE A GOOD REFERANCE TO YOU .

ASTM A216 : IT HAS THREE GRADE AS WCA,WCB&WCC ,IT COVERS CARBON STEEL CASTINGS FOR VALVES, FLANGES,FITTINGS FOR HIGH TEMPERATURE SERVICE .

GR. WCA GR.WCB GR.WCC

YIELD POINT 30000 36000 40000

MIN (PSI)
 
Check Chemicl engineering Hand Book (Perry) this gives usability of various material in various media. WCB is a common CS material, if you could get hold of ASME Sec II D then you could get the allowable stresses at different temperatures for designing purpose. Also ANSI B 31.3 could provide you with necessary information.

If you do not have Chemical Engineering Hand Book give the application i'll try to look and post you.