SUTA
Materials
- Dec 24, 2014
- 3
We are buying LCC ball valves. One manufacture offered 4140+ENP for Ball & Stem. Our MDMT is -45C. Would you please advise if the offered material is suitable for low temperatures?
Thanks in advance.