Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

STUD BOLTS ASTM A193 B7 - PMI

Status
Not open for further replies.

chrysa1975

Materials
Nov 14, 2007
64
ASTM A193 B7 IS CONSIDERED HIGH STRENGTH LOW ALLOY (MICROALLOYED) STEEL. STUD BOLTS B7 REQUIRE PMI (POSITIVE MATERIAL IDENTIFICATION)? THANKS IN ADVANCE!
 
Replies continue below

Recommended for you

Positive Material Identification (PMI) is normally specified as a Quality Control measure to verify material identification. As far as a Code and Standards requirement, no, there is no such requirement. You, as the user, can specify PMI prior to installation.
 
yes, metengr is correct. PMI is specified by USER. Sometimes it is required, sometimes it isn't.
 
A bolt PMI would be a hardness check to verify comformnace with A193 requirements.
 
grampi1;
A hardness check is not PMI. It is a method to verify heat treatment in accordance with a specification, it does not sort material.
 
Of course hardness is not PMI. But what is important about low alloy studs is their strength range. Don't want too soft or too hard. PMI could be fine, but still be a failure waiting to happen if heat treatment was wrong.
 