Fizza453
Mechanical
- Jun 22, 2011
- 262
Connection is Stub on between tube and header.
Tube ID is 69.1 mm and hole diameter is header is 50 mm.
Code of construction is ASME Section I.
Joint is full penetration weld as per Figure PW-16.1(a) but without backing strip.
So there is a mismatch of tube ID and Hole ID 69.1-50=19.1 mm.
Is this joint is acceptable?
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
Tube ID is 69.1 mm and hole diameter is header is 50 mm.
Code of construction is ASME Section I.
Joint is full penetration weld as per Figure PW-16.1(a) but without backing strip.
So there is a mismatch of tube ID and Hole ID 69.1-50=19.1 mm.
Is this joint is acceptable?
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN