Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Structural Steel Pipe material around 1945 1

Status
Not open for further replies.

monopoly

Structural
Oct 29, 2006
28
We are working on an old refinery. The existing piperack was built in 1945 with Standard Oil Co. specs. We are unable to locate the spec.
By searching around, our best guess the material for steel pipe that time was either ASTM A53 or A7, the Fy= 35ksi.
Do you have AISC ASD 4th edition? I hope it's indicated in the AISC.
Thank you.
 
Replies continue below

Recommended for you

If you are a member of AISC, you have access to all of the historic Steel Construction Manuals (through the 7th edition) for free,
From what I see, the load tables for pipe columns specified that it is assumed the steel from which the pipe is made meets the properties of ASTM A7, if pipe is made from other steel safe loads should be suitably modified.

See below for A7 specified properties:
A7_snip_rkl5wz.jpg
 
A53 Grade A has a yield strength of 30,000 psi and ultimate of 48,000 psi, but I don't know to what extent it has been produced or used for structural purposes.
 