Structural column strength chart 1

Status
Not open for further replies.
Replies continue below

Recommended for you

That chart looks like Johnson buckling curves. These Johnson buckling charts are based on crippling strength and column length. Where did your chart come from?

 
johnson introduced a parabolic cut-off to the euler column curve ... these curves look a little more simplistic.

bruhn (probably niu too) has a complete section on column allowables, and how to generate them (it's not that hard)
 
looks like a 68ksi (fcy) steel ? (reverse calc'ing the Euler curve)

why would the welded section be twice as effective as non-welded ? ... heat-affected zone increasing the allowable ?, but wouldn't this benefit be localised to the weldment ?

i'll assume you know the euler equation.

the johnson curve, for short columns, is a parabola with a max. strength of fcy, and tangent to euler at 1/2*fcy
 
That chart is from Bruhn. Page C4.7. I wrote a FAQ on how to purchase a copy (see the Aircraft Forum).

There are "C" factors (end fixity) missing from the .GIF file you have.


Steven Fahey, CET
 