I have a situation where a furnace is operating at 1922F with 3/4" Sch40 tubes. The Boiler & Pressure Vessel Code publishes allowable stress values up to 1650F. Does anyone have a recommendation for finding allowable stress values above 1650F for SB-407 N08810 pipe?
 
Replies continue below

Recommended for you

Hwat design Code/Standard is the furnace designed to? I would look there first.
 