AliGrailly
Mechanical
plz see the Table S301.3.1 Generic Pipe Stress Model Input ( b31.3 ) it gives the stress value of material ( A106-B ) at 288 degree = 18.1 ksi or 125 mpa , based on interapolation from table A-1 or A-1M :
500 F 600 F
19 ksi 17.9ksi
result : ~18.45 ksi / 127mpa
what s wrong?

500 F 600 F
19 ksi 17.9ksi
result : ~18.45 ksi / 127mpa
what s wrong?