I apologise if this is obvious. I was having a discussion at work and someone said that back calculating stress from Young’s Modulus isn’t good practice. The problem is that the analyst has calculated the compressive stress from the deflection using sigma = (E x extension) / length. Does anyone know if this is good or bad practice?