I want to draw stress-strain curve for ST37 (mild steel).
Dose any body have this curve? If it is "2 or 3 or 4linear" , it's enough.
Thanks a lot
alif
 
If you mean ASTM A36 steel.
Here is the bi-linear engineering stress strain data.

STRESS STRAIN
36 KSI 0.0012
59 KSI 0.001966666