Nov 1, 2003 #1 alif Structural Joined Oct 17, 2003 Messages 3 Location IR Dear friends Hi I'm working by ansys 5.4 I want to draw stress-strain curve for ST37 (mild steel). Dose any body have this curve? If it is "2 or 3 or 4linear" , it's enough. Thanks a lot alif
Dear friends Hi I'm working by ansys 5.4 I want to draw stress-strain curve for ST37 (mild steel). Dose any body have this curve? If it is "2 or 3 or 4linear" , it's enough. Thanks a lot alif
Nov 2, 2003 #2 fsi Structural Joined Jul 22, 2003 Messages 46 Location US If you mean ASTM A36 steel. Here is the bi-linear engineering stress strain data. STRESS STRAIN 36 KSI 0.0012 59 KSI 0.001966666 fsi Upvote 0 Downvote
If you mean ASTM A36 steel. Here is the bi-linear engineering stress strain data. STRESS STRAIN 36 KSI 0.0012 59 KSI 0.001966666 fsi