1}as per our requirement head had to be cold formed and had to be stress relieved but vendor provided hot formed head and said stress relieving not required .
P no.1 & Group.1 hot forming temperature 600 to 900.
All I want to know is which part of code proves about this.
Kindly help me to know more about code.

2}I would also like to know maximum thickness difference between flange and nozzle neck that can be welded beveling to required minimum thickness. (as per code)
Kindly help

3}As per UG-16 minimum required thickness for pressure retaining components is 1.5 mm excluding corrosion allowance is this valid for vessels containing hydro carbons, also what should be minimum thickness for internal plates we use excluding corossion.(As per code)

since I am very much new to design and trying my best to understand code requirements , expect help of all experienced person ,
kindly help
 
Replies continue below

Recommended for you

1}as per our requirement head had to be cold formed and had to be stress relieved but vendor provided hot formed head and said stress relieving not required .
P no.1 & Group.1 hot forming temperature 600 to 900.
All I want to know is which part of code proves about this.
Kindly help me to know more about code.

Please review
UG-79 FORMING PRESSURE PARTS
(a) Limits are provided on cold working of all carbon
and low alloy steels, nonferrous alloys, high alloy steels,
and ferritic steels with tensile properties enhanced by
heat treatment [see UCS-79(d), UHA-44(a), UNF-79(a),
and UHT-79(a)(1)]. Forming strains or extreme fiber elongation
shall be determined by the equations in
Table UG-79-1.

2}I would also like to know maximum thickness difference between flange and nozzle neck that can be welded beveling to required minimum thickness. (as per code)
Kindly help

UG-44 FLANGES AND PIPE FITTINGS
UG-45 NOZZLE NECK THICKNESS

3}As per UG-16 minimum required thickness for pressure retaining components is 1.5 mm excluding corrosion allowance is this valid for vessels containing hydro carbons, also what should be minimum thickness for internal plates we use excluding corossion.

The designer determines the applicability of corrosion allowance. This is based on materials of construction and known or determined process corrosion rate. Internal plates are not pressure retaining and can be designed using other approaches or Section VIII, Div 1 as a guide.

The information above is provided for you to research and try to determine the answers on your own. This type of forum is not meant to provide detailed engineering consulting activities. Seek help from a reputable pressure vessel design engineering firm.

 
@Metengr
I have read above mentioned section's to find my answers,
1)but I couldn't find requirements for hot formed carbon steel heads in the sections mentioned above.
2)same for thickness difference acceptable between flange hub and nozzle neck that can be welded without beveling.

I am just asking for some clarifications on topics for which I am not getting a clear picture from code, when I m trying to find the answer

Kindly help
 