Does 530C then turn the oven off sound good to you ?
I think thats it

Thanks
123Cat
 
Replies continue below

Recommended for you

Al casting alloys are not usually stress relieved. One method is to heat to a minimum temperature of 345 C for 2-4 hours. Higher temperatures will result in more complete stress relief. Be careful of incipient melting with a 12% Si alloy if you use 530 C.
 