Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Stress Analysis of Powder Metal Parts

Status
Not open for further replies.

bach4343

Mechanical
Apr 2, 2002
3
I want to do some stress analysis on a powder metal part. Can I just run the analysis the way I would for a machined part and just substitute the modulus of elasticity and poisson's ratio of the powder metal material?
 
Replies continue below

Recommended for you

This depends on the PM material and the objectives of the analysis.
PM technology is capable of making parts with density close to the fully dense condition (>99%). As such the parts can be analysed in the same way as any other parts. You will need the appropriate failure criteria etc.
Some PM parts are made with much lower densities; this may be for economic reason, to reduce weight, to act as a filter, to enhance lubrication etc. These types of parts should be treated with more care. This does not mean that they cannot be analysed as homogenous material, just that you may need to justify what you are doing.