Hai,
In our company, a plastic compoent made up of 30-35% glass filled nylon 6.6 failed during endurance testing.
Hence it was decide to carryout stress analysis using Finite element method.To start simple, it was decide to carryout linear static analysis. Later on slowly increase the complexity of the problem.
First, I started collecting the data for this plastic material. The supplier specification mentioned the following properties,
Tensile strength,yield = 95-195 Mpa
compressive,yield strength = 16-152 Mpa
Flexural yield strength = 110-310 Mpa
Poisson's ratio = 0.35
Shear strength = 59-85 Mpa.
The property values are also available in
I have few questions in this regard
My first question is,I was surprised with low compressive strength.Whether plastic fail in compression?
My second question is what is the failure theory to be followed for the plastics! Someone was referring cauchy stress for plastics.I have not yet beginned search in this regard. I will do google search. If you have any useful information,please share.
My third question is there any text book dealing with Finite element analysis of plastics or else stress analysis and failure theory of plastics.
If so, please share the information.
Definitely Linear analysis mayn't suffice.I have to do non-linear analysis.I am planning to get stress-strain data from our material labaratory.
My fourth question, Plastic doesn't have infinite fatigue life like ferrous metals. Is there any source where I can get some data about S-N curve for this plastic.
Thanks for reading this thread.
Have a nice day...
Regards,
Logesh.E
In our company, a plastic compoent made up of 30-35% glass filled nylon 6.6 failed during endurance testing.
Hence it was decide to carryout stress analysis using Finite element method.To start simple, it was decide to carryout linear static analysis. Later on slowly increase the complexity of the problem.
First, I started collecting the data for this plastic material. The supplier specification mentioned the following properties,
Tensile strength,yield = 95-195 Mpa
compressive,yield strength = 16-152 Mpa
Flexural yield strength = 110-310 Mpa
Poisson's ratio = 0.35
Shear strength = 59-85 Mpa.
The property values are also available in
I have few questions in this regard
My first question is,I was surprised with low compressive strength.Whether plastic fail in compression?
My second question is what is the failure theory to be followed for the plastics! Someone was referring cauchy stress for plastics.I have not yet beginned search in this regard. I will do google search. If you have any useful information,please share.
My third question is there any text book dealing with Finite element analysis of plastics or else stress analysis and failure theory of plastics.
If so, please share the information.
Definitely Linear analysis mayn't suffice.I have to do non-linear analysis.I am planning to get stress-strain data from our material labaratory.
My fourth question, Plastic doesn't have infinite fatigue life like ferrous metals. Is there any source where I can get some data about S-N curve for this plastic.
Thanks for reading this thread.
Have a nice day...
Regards,
Logesh.E