Hi Experts,
I posted this elsewhere and got no answer. May be somebody here can help.
I have a piece of ceramic(E=270000 N/mm2) glued with a two component epoxy to another much softer material like brick ( E=14000 N/mm2). The brick is much bigger than ceramic as in the attached diagram.
compressive force is applied on the brick which will deform following to Hook's law.
How much of this strain will be on the ceramic piece? or what is the strain in the ceramic.
What role has the epoxy modulus of elasticity?
thank you for any help
Jabir