elastic modulus usually refer to the storage modulus for an elastic material. While a rubber is not a full elastic, if you can only input a scalar into CAE, I guess you may want to use the nominal modulus which is the root square average of the storage and complax ones.
E(nominal) = sqrt(G(storage)^2 + G(complex)^2)