I’m used to using fillet stitch weld of floor plates to the beams 1" long every 12". One of these things that this is how we do it in the company, and no one ever questioned it.
Recently I noticed section in AWS 2.3.2.4 calling for minimum 1-1/2" for intermittent fillet welds.
Does anyone know why min 1-1/2" is required if for structural purpose 1" is enough?
Also, why the same minimum length doesn’t apply to grove weld? Some of my plate will be welded to HSS, so I wanted to use stitch flare bevel grove weld also 1" every 12".
Any thoughts on that would be appreciated?