Stellite is normally applied with TIG welding, or spray coatings. The weld procedure would depend on the thickness and alloy content of the base metal it is being applied to. You may need to develop your own weld procedures, or hire a contractor.
Frank Moore, P.E.
Consulting Metallurgical Engineer
Kansas City Power and Light Co.