Anyone having a Descriptive Procedure on Stelliting, can you please show me the way?
Thanks
 
Is stelliting similar to PVD?
 
Stellite is normally applied with TIG welding, or spray coatings. The weld procedure would depend on the thickness and alloy content of the base metal it is being applied to. You may need to develop your own weld procedures, or hire a contractor.

Frank Moore, P.E.
Consulting Metallurgical Engineer
Kansas City Power and Light Co.
 
Stellite is a tradename for CoCr or CrCo alloys used in various applications. I have applied the material with SMAW, GTAW, and OFW. The various grades of stellite will have varying characteristics ad application techniques.

Thermadyne appears to now be the owner of Stoody. Here is a page with some informatiuon on various hardfacing products
Have a nice day


Gerald Austin
Iuka, Mississippi
 