There are stories here of a crusher shaft that(1) bent in service or (2) had a low natural frequency. The steel reportedly test OK chemically, but demonstrated low modulus during some physical tests.
I'm trying to find out more, but in my mind I'm clutching to the Bauschinger effect as a >>possible<< explanation. Is it possible if the test sample was cut from a peculiarly yielded piece of the shaft an odd, low modulus might be measured?
Thanks,
Dan T
I'm trying to find out more, but in my mind I'm clutching to the Bauschinger effect as a >>possible<< explanation. Is it possible if the test sample was cut from a peculiarly yielded piece of the shaft an odd, low modulus might be measured?