MiketheEngineer
Structural
This may not be the best forum but one thing I know - you guys have seen it all and respond quickly.
I have a primed steel to aluminum connection on interior of building. So it will always be dry. I have no trouble with the connection design - but now the owner is worried about corrosion or galvanic action or whatever.
I don't believe this to be a problem - at least for the next 100 years or so. Your thoughts please.
I have a primed steel to aluminum connection on interior of building. So it will always be dry. I have no trouble with the connection design - but now the owner is worried about corrosion or galvanic action or whatever.
I don't believe this to be a problem - at least for the next 100 years or so. Your thoughts please.