Hello,

I need the specs. of the steel A48, A48 M and A 48 M2 (French AFNOR Standards).
But I could not find the name of the standard about these steel types.
Does anybody know which standars refer to these 3 types of steel?

Thanks in Advance
 
I don't have a reference to those specific grades, but you should try NF A36-205 and NF A36-601, which list other grades of A48 steel.
 