Thank you all.
We are brazed tungsten carbide people and definitely not steel people. In some saw blades they cut slots in the body and braze in strob strips that are the width of the saw teeth. These serve to move the sawdust out of the cut and to help center the saw blades.
The company that used to sell these in steel no longer does. They are available in carbide but steel is preferable since the saw bodies flex.
These parts are brazed in using braze alloys (filler metals ) that work at about 1300 F see:
Currently the customer is cutting them out of old M2 knives using an abrasive wheel. We have done the same and this is not a good project.
Ideally we would have a steel that is easy to cut and that will be hard after we braze it on at 1300F.
0186 from Sharon steel and Boron steel called Tuff Steel form Plaanja have been recommended from one source. Another source recommended 1090. As I understood it the 1090 should be readily available and have the ability to retain sharp edges under wear even after brazing.
We currently have an order for 500 parts .125” x .155” x 2.00” in whatever steel we recommend.
We would like to help a customer and this could be a nice, small product line but we are definitely not steel people.
Thanks,
Tom
P.S. Since they drastically reduced exposure limits for Cadmium its use in braze alloys has dropped precipitously but there are other braze alloys.
Thomas J. Walz
Carbide Processors, Inc.