Mar 7, 2018 #1 Viekku Materials Joined Mar 7, 2018 Messages 1 Location FI Hi all! I wonder what letter S (without any number) means after grade name in A516 Grade 60S?
Mar 14, 2018 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Typically, there is no alpha suffix designation after the ASTM A 516 Grade minimum tensile strength level. Upvote 0 Downvote
Typically, there is no alpha suffix designation after the ASTM A 516 Grade minimum tensile strength level.
Mar 14, 2018 #3 EdStainless Materials Joined May 20, 2004 Messages 16,348 Location Waukesha WI USA If there was a number following the 'S' it would refer to a supplemental requirement. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
If there was a number following the 'S' it would refer to a supplemental requirement. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube