Hi all!
I wonder what letter S (without any number) means after grade name in A516 Grade 60S?
 
Typically, there is no alpha suffix designation after the ASTM A 516 Grade minimum tensile strength level.
 
If there was a number following the 'S' it would refer to a supplemental requirement.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 