Hello all,
I am about to embark on a new manufacturing endeavour, and would like the help and advice of knowlegeable members:
I will be building rifle actions. I have all of the materials specified by the designer/metalurgist. The main body is plain 4140 in pre-hardened state, post ionic nitrided and finished with some other treatment for asthetics (likely cold bath bluing). The bolt body, is however, being a pain to find material for.
The material is 36nicrmo16 (1.6773), and obviously, there is no AISI/BS etc equivalent, although AISI 4340 seems to have some relevance. The bolt body is to be heat treated to 52 HRC. It has internal holes bored on center for firing pin mechanism etc, and is probably on average two thirds its radius in thickness. Overall length about 5 1/2 inches, diameter about 1 inch
What other steels have a similar makeup, or similar end properties that people here may know of? What suppliers have this material? Are there any people here in Australia that know of suppliers? I have had a number of conversations with Bohler Udd. with no success so far (except 4340 that they don't have in stock anyway).
Regards
woodyrod
I am about to embark on a new manufacturing endeavour, and would like the help and advice of knowlegeable members:
I will be building rifle actions. I have all of the materials specified by the designer/metalurgist. The main body is plain 4140 in pre-hardened state, post ionic nitrided and finished with some other treatment for asthetics (likely cold bath bluing). The bolt body, is however, being a pain to find material for.
The material is 36nicrmo16 (1.6773), and obviously, there is no AISI/BS etc equivalent, although AISI 4340 seems to have some relevance. The bolt body is to be heat treated to 52 HRC. It has internal holes bored on center for firing pin mechanism etc, and is probably on average two thirds its radius in thickness. Overall length about 5 1/2 inches, diameter about 1 inch
What other steels have a similar makeup, or similar end properties that people here may know of? What suppliers have this material? Are there any people here in Australia that know of suppliers? I have had a number of conversations with Bohler Udd. with no success so far (except 4340 that they don't have in stock anyway).
Regards
woodyrod