Steel call out on drawing 1

Status
Not open for further replies.

dougbevi

Materials
Nov 18, 2008
3
I'm having trouble finding this for one of my customers and a material call out they need for a washer.They are requesting SPC590 for the part. They were using DC01-C490 but changed the spec to a SPC590. My manufacture has no idea what the spec is and I need an answer to clarify my manufacturer as well as my customer.Any ideas anyone
 
Replies continue below

Recommended for you

SPC 590 is a partial designation from Japanese-based steel standards.

S = steel
P = plate (actually sheet, while other forms would be bar, wire, tube, etc.)
C = cold rolled
590 = minimum ultimate tensile strength in MPa

Here is one of many products that are in this class:


DC01 is a partial designation from Euronorm steel standards.

D = flat products for cold forming
C = cold rolled
01 = code for mechanical properties

You need to obtain full specifications of the materials to move forward.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks Cory for the info I will pass it along to my customer

Doug
 
The real designation is SPFC590 according to JIS G 3135. As CoryPad mentioned it is a high yield strength steel typically used in automotive forming. JFE Steel is a Japanese producer of this type of steel (their version is called JFE-CA590). Check out pages 5-9 of the following .pdf file for more information:

 