Gopher13
Structural
- Jun 21, 2016
- 94
I have a question about bearing plates for steel lintels over openings is cmu walls. Should the bearing plate sit on the face shells or should it just sit on the grouted core? In my case, they will be cutting an opening is an existing cmu wall. I am requiring them to grout three cores below each bearing point. If the bearing plate is sized so that it only bears on the grout then I am relying on the bond between the grout and the mortar to hold up the lintel (this seems worrisome to me), however if I size the lintel to bear on the face shells there will not be a full bed of mortar.
All comment would be helpful. Thanks in advance!
All comment would be helpful. Thanks in advance!