mavericktim89
Industrial
Hi, I'm working in a Steel Bar Rolling Mill and we produce steel bars for construction. Lately I'm problems with the Yield Strength of the finished products. The YS has a very large difference between the head and tail of the product. I have tried a few things to arrest this problem:
1. Increase/maintain the pinching of the pinch roller and control it's speed
2. Adjusting the cooling box water flow rate and pressure
3. Maintaining a uniform bar diameter throughout the whole product (consistent tolerance)
However the problem still exists. What else I can think of is:
1. Raw material chemical composition problem
2. Under heat raw material in furnace
Has anyone had this problem before?
1. Increase/maintain the pinching of the pinch roller and control it's speed
2. Adjusting the cooling box water flow rate and pressure
3. Maintaining a uniform bar diameter throughout the whole product (consistent tolerance)
However the problem still exists. What else I can think of is:
1. Raw material chemical composition problem
2. Under heat raw material in furnace
Has anyone had this problem before?