Hello to all,
Well, this is my first post.
I'm a mechanical engineer with ~10 years experience.
Each time I have a steel selection to do, I have a real hard time finding a "commonly available" type of steel (with a required yield strenght, for example) versus the shape required.
For example (but not actual questions):
- Is 4140 available in 6" round bars?
- Is A572 GR 80 available in 1" plate?
I believe at some point it is the same question every mechanical engineer has when choosing a material (Required specs VS availability VS price).
Does anyone have tips on material selection VS availability? A book to suggest? A program? A website?
Thank you very much
Well, this is my first post.
I'm a mechanical engineer with ~10 years experience.
Each time I have a steel selection to do, I have a real hard time finding a "commonly available" type of steel (with a required yield strenght, for example) versus the shape required.
For example (but not actual questions):
- Is 4140 available in 6" round bars?
- Is A572 GR 80 available in 1" plate?
I believe at some point it is the same question every mechanical engineer has when choosing a material (Required specs VS availability VS price).
Does anyone have tips on material selection VS availability? A book to suggest? A program? A website?
Thank you very much